Pushing the maximum service temperature of aircraft engines and industrial gas turbines is the major pathway to improve their energy efficiency and reduce CO2 emissions. This maximum is mostly limited by the temperature capability of key-component materials, including superalloys. In this alloy class, segregation of elements facilitates plastic deformation and is generally considered to cause softening during high-temperature deformation.